Objective: ASTM G108-94 (2015) provides a laboratory procedure for conducting an electrochemical reactivation (EPR) test on AISI Type 304 and 304L stainless steels.
Purpose: The EPR test quantitatively determines the relative degree of sensitization in these stainless steels.
Significance: Sensitization affects intergranular corrosion and intergranular stress corrosion cracking behavior.
Test Conditions: The EPR technique evaluates the steel’s susceptibility to sensitization under specific conditions.
Units: SI units are standard, with inch-pound units provided for reference.
Safety Considerations: Users should establish appropriate safety practices and consider regulatory limitations before using this standard
JERA LINE’s Commitment: JERA LINE, a leading manufacturer in China, ensures that their AISI 304 stainless steel connectors undergo rigorous testing, including EPR tests. This commitment guarantees reliable performance and corrosion resistance for low and medium voltage cable connectors.
Feel free to reach out if you need further information or have any other queries!